Source for 6mm PCD router bit
5/13/17
Hi all
Did anyone ever come across a supplier for small diameter pcd router bits. I'm using both expensive, and cheap Chinese carbide cutting aluminium dibond, foamex and sheet materials.
I'm fed up changing and calibrating 6mm bits.
I get long life nesting with 16mm pcd (maybe 500 sheets MDF or 300 sheets MFC)
5/13/17 #2: Source for 6mm PCD router bit ...
How deep are you cutting? I'm using a 3/8" diameter, 2 flute PCD bit from Leuco with a slight downshear angle.
The cutting length is only about 1/2" though.
5/14/17 #4: Source for 6mm PCD router bit ...
Thx Gary b
60% 3mm dibond
30% 10 mm foamex
10% 19mm foamex
The letters are most times small < 50mm so a 6mm bit is the largest diameter I can go.
Sometimes a 3mm would work best but I'd say it would be pointless looking for a pcd 3mm with 20mm LOC
5/15/17 #5: Source for 6mm PCD router bit ...
Website: http://www.vortextool.com
Mick- We offer a two flute PCD cutter in 1/4"CED x 1/2" CEL, if that would work for you. Part number 6730
5/15/17 #6: Source for 6mm PCD router bit ...
Mike S
I'd say that would get me out of trouble but I don't see it in your catalogue.
Can you invoice me to demfolshopfit@gmail.com inc postage to Ireland and I'll arrange payment.
Regards
Mick Folan