Injecting glue into dowel holes

7/10/19       
Oggie Member

Just starting with dowel construction for cabinet cases and looking for entry level solution for injecting glue into dowel holes.

Searching through older post I've found that Lamello used to make some manual glue dispenser called "Lamello Dosicol 177007", but can't find it any more, only some similar with nozzles for biscuits.

Also, pressurized pots like Lamello LK-3 are not out of range (would like to stay under $1K), but I've never used one of those and can't figure out from scarce Youtube videos if it's any good for that specific purpose (is there some preset quantity of glue that will be injected with each squeeze of the handle or the flow is continuous and you just develop a feel for the right amount of squeezing time)...

If we leave dedicated dowel and glue inserter machines out of scope for now - what other methods/gadgets/systems you use to insert glue into dowel holes?

Thank you

7/10/19       #2: Injecting glue into dowel holes ...
KCR

Go to this link: https://www.csaw.com/lamello/glue-systems/
I have been using it for about 25 years. It was developed by a company called Schnieberger (spelling ?) and later purchased by Lamello. Exclusively sold through Colonial Saw. I love this system and use a variety of tip designs including a custom tip I use for glueing 1/4" x 1 x 1 1/2" loose tennons for assembling faceframes, edgeglueing solid panel stock, broad surface laminating, etc. To be sure, it is pricey but for all the options it offers, it really speeds up all of the glueing process for a one man shop!

7/10/19       #3: Injecting glue into dowel holes ...
Oggie Member

So, that would be that Lamello LK-3/5/10 I mentioned above... Can be bought at Home Depot or Amazon too.
It looks well suited for a variety of gluing applications but I am interested in one and only one - inserting glue into dowel holes.
Do you think it's good for that? Can you set a precise amount of glue that will be delivered into the hole with each push on a gun's lever?

7/10/19       #4: Injecting glue into dowel holes ...
Alan F. Member

Little more expensive but what we use

https://www.tritec.com/copy-of-semi-automatic-glue-and-dow

7/10/19       #5: Injecting glue into dowel holes ...
KCR

I had no idea you could purchase this equipment through Home Depot!
To your question, yes. It's GREAT for that!They have a special device LK 100 or LK110 that dispenses a regulated amount of glue for a set length of time (fractions of a second or two). Be sure to read through the website or call them to get precise info on your needs.

7/10/19       #6: Injecting glue into dowel holes ...
Oggie Member

So, I've made a few phone calls and got some pricing. LK-3 basic system has a "manual gun" - the glue flows as long as you keep the handle pressed. But it has flow adjustment so you can reduce the flow in order to increase resolution on your timing. I suppose one could develop a feel for right duration of squeeze relatively quickly.
The gun that injects the measured amount of glue with each stroke ("One-Shot" model) unfortunately costs alone as much as twice than the basic system complete, so that one is out of scope for now.

Also, the glue that will work with this system is regular viscosity (Titebond) wood glue and not low(er) viscosity dowel glues used with specialized dowel and glue inserter machines. Don't know why, but that's what I've been told.

7/10/19       #7: Injecting glue into dowel holes ...
chris barnard

check out this.

Rangate - Pizzi glue system

7/10/19       #8: Injecting glue into dowel holes ...
Oggie Member

Looks very similar to Lamello.

As a matter of fact, the more I look into how these are made the more I'm closer to conclusion that a $100 pressure paint tank from Harbor Freight and a $10 air blow gun with a few feet of hose would work the same, except for the nozzles, but they are not included in those more expensive systems either.

7/10/19       #9: Injecting glue into dowel holes ...
Bruce H

I have a Schneeberger same as KCR, more than thirty years. It's easy to dispense the right amount of glue into a dowel hole using a manual gun. I have dowel tips for 5mm, 8mm, 10mm, 1/2" and also have tips for everything else. It's the "cats meow" when it comes to inserting glue into dowel holes or gluing anything else. I put a gallon bottle of glue in the tank and leave it until it's empty, no cleaning. I do keep the gun in a pail of water.

7/10/19       #10: Injecting glue into dowel holes ...
KCR

If you decide to go with the Lamello system you will also want to get a cleaning adapter for a slop sink. It screws on to the end of the faucet and allows you to attach the various nozels from the gun and rinse the glue out of them before storing them. I have always had my tips in a bucket of water and it caused the tips to deteriorate. Wouldn't do that again.

7/12/19       #11: Injecting glue into dowel holes ...
Alan F. Member

this has the tank and nozzle; seems like a good price

http://machinerymax.com/Event/LotDetails/16385713/Pizzi-Glue-Table

7/13/19       #12: Injecting glue into dowel holes ...
Ken Member

Here's another supplier of gluing equipment. https://vansco.com/catalog/

7/15/19       #13: Injecting glue into dowel holes ...
Dan Dempsey Member

Website: CSaw.com

Hi everyone, lots of good feedback here, just wanted to chime in as well on behalf of the crew here at Lamello USA. We have lots of guys using our LK One Shot systems for dowel assembly throughout the US. In fact, some machine manufacturing companies sell the LK systems in tandem with their case clamps.

Most shops that are using the system for dowels will opt to go with the One Shot system- they want to be able to ensure the exact same amount of glue is being inserted each time they hit the trigger. That being said, these are shops where they don't necessarily have their most skilled employee inserting glue for the dowels, so they need to have that level of control. Oggie is correct in thinking that you'll develop a "touch" for how long you need to hold down the trigger to get the right amount of glue. As a few of you have pointed out, these systems are well built machines and with some basic maintenance, will last for years.

If you were to decide later on that the pneumatic One Shot was a better fit for your application, you can always buy the pneumatic set-up at a later time. Hope this helps!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello