1mm White PVC Edgeband
4/15/17
Decent source for this? We've been getting it from Richelieu for years, but have been increasingly less satisfied with the quality.
Looking for alternative sources. Thanks.
4/16/17 #3: 1mm White PVC Edgeband ...
Website: mcgrewwoodwork.com
Charter industries, framatech, edgeco,
4/16/17 #4: 1mm White PVC Edgeband ...
Thanks, I should say alternate/economical source. We go through a fair amount of this and I've found that the price can vary widely.
4/16/17 #5: 1mm White PVC Edgeband ...
You might want to post what part of the country you are in, since freight is a significant factor in banding cost if not bought with free shipping. I bought 1 MM white PVC from these people located north of Chicago.
http://pri-edgebanding.com/
4/16/17 #6: 1mm White PVC Edgeband ...
Located in Northeast. Thanks for the link.
4/22/17 #7: 1mm White PVC Edgeband ...
DC Distributing
800-727-0917
in PA
edgebanding is all they do
4/22/17 #8: 1mm White PVC Edgeband ...
As Rich suggeted, it's looking as though shipping may be a deciding factor. Do any of these companies offer free, or a flat cost for shipping. We typically order 15 rolls at a time.
4/23/17 #9: 1mm White PVC Edgeband ...
Edgeco is by far the cheapest. Im in California and buy from them. They have good price breaks for volume, quality is very good.
Side note, make sure you rotate your stock. We had a few rolls at the bottom of the stack that hadnt been used and was over 1 year old qnd had become brittle and not usable.