Press for laminations

5/18/18       
Craig Caughlan Member

Website: wetimber.mx

I'm wanting to fabricate a press for rails and stiles that would probably use modified bar clamps for economy.

What I'm primarily wanting to glue-up in one pass for instance are five sets of three sticks
that are 1"x4" x 10' long.

What would be great is if I could construct something that I could also use for beams and columns (glu-lams of larger material).

I'm curious as to what others have for this purpose and would welcome photos of your shop-made press.

5/21/18       #2: Press for laminations ...
David R Sochar Member

In the first real shop I worked, they had an 18' long glue up 'table' for handrail laminating. 2 x 4 horizontal struts, White Oak, coming out from the wall about 24". 45 degree angle 2 x 4 struts below to the wall for support. These were about 8" on center, and leveled very accurately, with long straightedges. About 12" from the back wall was a 2" thick x 3" tall hardwood running the 18'. It was lagged to the Oak struts and made a good 90 degree face. Everything was waxed with Gulf Paraffin cakes.

It was used for the lamination to thickness of multi-ply handrails. A dead-stop at one end enabled pushing the various butt joints together as it was clamped. We used handscrews to clamp the laminations to every strut. And then a handscrew was used to tag the laminations tight to to the 2 x 3 spine to keep it all in line - and straight.

This had several drawbacks - slow to clamp. Needed a caul on top to help distribute the clamping force. Slow to cure with 'yaller' glue. Could only do one rail at a time. Big clean up on the struts between parts. Glued some parts to the back rail or spine. Wax would get everywhere, not always a good thing with wood.

We fantasized about air clamps overhead, each with a 12" long 8/4 caul to distribute pressure and a control valve on each. Iron angle struts to minimize contact and make clean up easy. And some sort of plastic face on the 18' spine to repel glue. But the shop closed long before any of that happened.

In subsequent shops, we have made straight rail many times, up to 28', but we never felt the need for such an apparatus. A good eye and properly prepared stock kept everything in line. We do use benches (all meticulously the same height) for long, straight glue ups, but a good eye still is needed.

Today. I would do this on the 9' bench, stacking and gluing and make one tall stack, sitting on equal thickness blocks on the bench to hold the clamp handles off the bench. Clamp it with pipe clamps opposite sides, about every 8-10". Let it cure. I will buy you lunch if they are not all dead straight - assuming you prepped the material properly - faced and edged on the jointer and then planed.

5/22/18       #3: Press for laminations ...
Craig Caughlan Member

Website: wetimber.mx

What you described in your last paragraph is what we're doing now on 10' tables.

I was thinking of doing something like what you described in your first paragraph, using one of our long walls, and moving to some kind of "bench" set-up and get off the tables.

I too like air and hydraulics, but I'd like to keep it simple. I'd like to get away from using so many clamps - maybe a steel caul with a slight curve, laminate-faced.

I'm also starting to think RF for the volume I might need.

Thanks Dave for taking the time to respond,

5/22/18       #4: Press for laminations ...
David R Sochar Member

It is all about volume. Enough of those things and the pneumatic cylinders get more attractive. They would squeeze out the glue, then keep the pressure on. Pipe clamps may have XXXX lbs of clamp force when first tightened, but that could drop to XXX after some of the glue has drained out.

It would be nice to have the rack, but maybe two sided, and with shorter clamps (most of mine are 42" min, up to 52" or 100" - hard to stick up in the air). Two people, working together should be able to run 5-6 parts in about 30 mins. 2-3 hrs later, and change them around.

I got an idea. Why don't you do some experimenting on your project, and post back and let us know what you learned. Then we don't have to go spending time and money on half a system.

Best of luck on it.

7/15/18       #5: Press for laminations ...
Craig Caughlan Member

Website: wetimber.mx

I thought I'd followup on my search for ideas on a press to laminate boards by showing what I've done so far.

It's a work in progress. We can laminate up to 12' long sticks. Wanting consistency, we're using a torque wrench at 25 ft lbs, probably about a full turn more than what you would do with a hand clamp.

As you can see, we have to beef up the tube steel clamps on the 'X' axis. It might be better to have two-points rather than a single in the middle, but a factor in the decision to keep it in the middle was reducing the open time of the Tite Bond III.

There are other changes that need to be made; it's not the end result of what we need, but it's a good starting point.


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery