Residue-Free Labels Latest in Tools and Supplies

What Glue Bonds Pb Edge To A Melamine Face.

06/15/2012


From original questioner:

I need to make melamine shelves with a 2" skirt around the the front and 2 sides. The melamine is pb core and all material is .75"
I plan on constructing the shelves by gluing the 1.25" skirt to the underside if the .75 main shelf. I have seen it done where the pb and melamine are bonded directly together without cutting the melamine face off and the joints I have seen seem to be quite strong and more then adequate for the application.
I'm not sure which glue to use for this. I was going to try the hi-pur glues first.

From contributor Jo


See link below:

From contributor Ad


Roo

From contributor La


Franklin's melamine glue. White in the jug, dries clear, works great. Same company makes Titebond

From contributor Mi


What you need is Spectrum Adhesive/CP Adhesive Melamine Plus adhesive.

Works better than a melamine glue for this application.