Using D.B.H. and Butt Log Quality to Estimate Tree Yields by Saw Log Grade

Presents a shortcut method of predicting sugar maple tree yields by saw log grade from d.b.h. and butt log grade. 1968
This article is in PDF format (file size: 473 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Using D.B.H. and Butt Log Quality to Estimate Tree Yields by Saw Log Grade   (1968)

Presents a shortcut method of predicting sugar maple tree yields by saw log grade from d.b.h. and butt log grade.

Author: Hyvarinen, Matti J.


Source: Research Note NC-67. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Hyvarinen, Matti J.  1968.  Using D.B.H. and Butt Log Quality to Estimate Tree Yields by Saw Log Grade  Research Note NC-67. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.