Use Hardwoods for Building Components
Other Versions
Spanish
French
Describes a system for prefabricating structural units from hardwoods for use in floors, roofs, and walls of a-frame or post-and-beam type construction. The interior face of the unit is decorative paneling; the exterior face is sheathing. Use of the system could reduce prefabricated house construction costs compared to conventional construction costs. 1968
This article is in PDF format (file size: 942 kb).
To download this article, right click on the link immediately below
and choose "save target as". To view the article, left click the link
immediately below.
(Download the latest
Acrobat Reader if required.)
Use Hardwoods for Building Components (1968)
Describes a system for prefabricating structural units from hardwoods for use in floors, roofs, and walls of a-frame or post-and-beam type construction. The interior face of the unit is decorative paneling; the exterior face is sheathing. Use of the system could reduce prefabricated house construction costs compared to conventional construction costs.
Author: Cooper, Glenn A.; Rice, William W.
Source: Research Note NC-46. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station
Citation: Cooper, Glenn A.; Rice, William W. 1968. Use Hardwoods for Building Components Research Note NC-46. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.