Preventing Animal Damage   (1988)



Author: Weber, Barbara C.; Van Sambeek, J. W.


Source: Weber, Barbara C.; Van Sambeek, J. W. 1988. Preventing Animal Damage. In Burde, E. Lucy, ed. Walnut Notes. St. Paul, MN. U.S. Department of Agriculture, Forest Service, North Central Forest Experiment Station. : Note 5.06.

Citation: Weber, Barbara C.; Van Sambeek, J. W.  1988.  Preventing Animal Damage  Weber, Barbara C.; Van Sambeek, J. W. 1988. Preventing Animal Damage. In Burde, E. Lucy, ed. Walnut Notes. St. Paul, MN. U.S. Department of Agriculture, Forest Service, North Central Forest Experiment Station. : Note 5.06..