Residue-Free Labels Latest in Tools and Supplies

Panel and Door Balancing with 32mm Systems

A closet contractor struggles to make his standardized shop system compatible with specs for a commercial job. September 30, 2010

Question
I was wondering if anyone can enlighten me on the 32 mm system. We cut closet parts for a few closet companies in our area. We start the first 5mm hole 9.5mm from the edge of the panel on the top and bottom edges. That way the panel is balanced. So when an 84" panel is specified, we have to cut it at actually 83.9 inches to achieve balance.

So, our first commercial job comes up. Architect's drawings specify standard 34.5" base with 4" toe kick (30.5" end panel). Fine, but with our closet system standard of starting and ending the holes at 9.5mm, we now need to cut a 30.5" base end panel at something like 30.875 in order to keep balance. Is it understood in the commercial industry that specified sizes might change in order to accommodate the 32 mm system, or am I way off base and somehow need to develop a system where I can cut the panel to 30.5 and still keep the panel balanced?

Forum Responses
(Cabinetmaking Forum)
From contributor R:
There are several good 32mm systems, so reinventing your own is not a good use of time. I always thought a balanced panel was referring to the door where the hinge holes were bored the same distance from the top and bottom. Then they are not handed. And shelf holes are always bored from the bottom.

The cabinets do have to be a certain height to get a balanced door, but the holes are not balanced on the sides. My doors then are flush on the bottom of the cabinet and 10mm below the top of the cabinet. This gives a balanced door. And whatever a designer says, you are the cabinetmaker. You build your way to ensure the cabinets meet code. In California that is ADA.



From contributor J:
Our first hole is different than yours, but we cut our side panels at 774 or 30.472. This give us balanced panels and keeps standard heights. We use adjustable levelers for our 4'' toe, which will only be 4'' at one point anyway due to out of level floors.


From contributor M:

My gables (line boring) are not balanced. I keep my doors balanced, but do not worry about the side panels.

Most designers or architects will be okay with minor adjustments, but ask first. I offer my standard sizes in 32mm height increments. I can usually adjust the toe kick 16mm up or down to cover the difference on lower and tall cabs. If the client is insistent I can alter the top and bottom a few mm. Worst case scenario is I have to deal with unbalanced doors. In reality the changes on the boring have almost no effect on my production, and I am using 21 and 23 spindle boring machines, not CNC. What machines are you using to bore the panels?



From contributor S:
Standard base and upper side gables, 768 mm, 30 1/4", makes things simple. Inform your client that this is your system. I keep the mindset that architectural drawings are for concept, not production. As long as everyone is in the loop there should be no issue. If they are that picky, ask to have the floors dead level and walls plumb. As we all know, that will never happen. Variances in these two factors are greater than any sizing difference.


From contributor E:
Visit www.true32.com and snoop around. These guys have the best published 32mm system in my opinion. The book and video may be the best $100 you spend if you want to do 32mm cabinets.


From contributor M:
One of the reasons for drilling vertical panels balanced is that the panel can be reversible. There is no designated top or bottom. In some cases, based on equipment and your drilling process, this can simplify things. It can also be helpful in the field in doing installations. On the other hand, it may not be that beneficial at all. The biggest impact would be that if you drill as you normally do, the people in the field may be expecting a balanced panel, but then they may not. I often buy from a closet supplier that likes to do everything using the balanced verticals, even though we don't have to have them this way. Sometimes I need a vertical a certain length due to the conditions found in the field. I tell my closet supplier to override his system, and I will deal with the unbalanced drilling on my end. Usually all it means is the very top hole will be a little closer or further from the end. The only time it would concern me is if I were doing a full drawer stack with a short vertical, or if the top holes were being used to attach a cabinet door hinge.

Then it can affect how the top of the drawer front aligns with the shelf above or the cabinet top. Also it will matter with cabinet doors if they are being hinged in the top holes using the 32mm system. It depends a lot on how the particular system has been designed.



From contributor Y:
Do what contributor J said (true32.com) and don't look back except to see your bank account grow as you become business focused and forget wasting time and money trying to reinvent the wheel.


From contributor I:
Another vote in favor of buying the True32 book.


From the original questioner:
Thanks all for the responses. I will be machining all parts on an Omnitech CNC. Based on the responses and what I have researched on the net, there isn't one system to use. Everyone has their own little way of doing it. The system we use for closets will get us close to the standard US inch increments but obviously not right on because it is in millimeters and in multiples of 32mm. I think I will just spec it out using our current way and bring a sample along showing the GC and client why our measurements will be slightly larger or smaller that the spec'd architect inch drawings. My brain is so racked right now trying to figure out something that should be so easy. Does anyone know of a web site that lists all of the panel sizes that can be used in the 32mm system along with the standard drawer front and door sizes?


From contributor E:
www.true32.com. Buy the book. Buy the video.


From contributor R:
Here is the manual for Blum's Process32 system. Has all the sizes you need.

Blums_Process_32_Manual_PDF.html">Blum Manual



From contributor D:
If you are using the 32mm system and 9.5mm top/bottom starts, you are making half-overlay cabinets using 19mm stock (11mm perimeter reveal). Doing that is great for closets where you can stick doors or drawers anywhere and all horizontal panels center on system holes. You probably want a full overlay panel design for your commercial job.

Contributor R, there are balanced panels and balanced faces. The 32mm system requires balanced faces, but not balanced panels. Having your faces flush to the bottom of the box requires using unbalanced panels.

Contributor J, if you are using the 32mm system and your 774mm panels are balanced, you have a 3mm top and bottom reveal on your cabinets (assuming 3mm field reveals).

Contributor M, I agree with the concept of doing a +/- on the toe-kick; there is no reason a toe-kick has to be, or can be (end to end of a run), 4" exactly.

Contributor S, your 768 mm panel is divisible by 32mm and is either balanced with 1.5mm top and bottom reveal or unbalanced with a 3mm top and 0mm bottom reveal (assuming 3mm field reveals). It's a standard full-overlay stackable box design, the one used by the True32 folks.

To the original questioner: there really is just one 32mm system. To be able to use the system holes to index components, all face heights plus reveal must be divisible by 32mm (full/half overlay and no rail inset designs). The differences in 32mm designs have to do with the top and bottom face to panel reveals and if the face edges center on or between system holes. Full overlay panel sizes: Kiss = 32 x n + 6mm, Process32 = 32 x n + 7mm, Proulx and True32 = 32 x n.


Click here for higher quality, full size image



From contributor T:
Visit True32.com, easily the best professional site around, become a sponge, and study, study, study. With CNC it's arguable to some whether you need a system or not. I think to get a repeatable grip of design you need a system, which means things built in height increments of 32mm. Kick and mold provides wiggle room. Width and depth can be anything.


From contributor M:
I too have the True 32 book, and it is a great introduction to the 32mm system. Not only that but he covers a lot of other important ideas like panel choices and production flow. But it is not the best for everyone and is a little dated. Look at the KISS and KISS2 system. And Blum's system is also really great. It takes a lot of thought to come up with a perfect system and even then you will likely change it as you buy new machines and gain experience. Even the software you use is a huge consideration. Not many programs are 32mm friendly. I will say that Cabinet Vision is the best I have seen in this area.

Balanced panels only really matter if you use manual boring equipment and line bore every hole in the pattern. And for most situations even reveals top and bottom are bad. For example I want my uppers to have 0 reveal on the bottom and a 3mm on top. This way there is no edgeband stripe under the doors and if I add a cap or crown to the top the top gap is already correct. My base cabinets have a 4.5mm reveal on top and 1.5 on the bottom. This way I can still use slides that ramp up when the drawer is opened, and the doors do not get damaged when sliding the cabs on the bench or floor. For stacked cabinets I use 1.5mm top and bottom.

This creates unbalanced panels but the doors and drawers are balanced and the reveals/gaps always split a system hole. I use manual boring machines and the only setting we change is the offset for the first hole location (uppers have no offset). The machines do not care how tall the panel is. All the operator has to do is drop the bits into the correct spindles based on the indicated pattern. My internal cabinet names include all the boring information the operators need.

Like others said, if you are using CNC, it doesn't matter very much. It is still good to keep doors balanced and to keep things like the drawer false front reference the same. But I still think a CNC has a hard time competing with a 32mm shop using a good system. What we can do in one day with three or four guys is pretty darn amazing and my equipment was 1/3 to 1/4 the cost of a good CNC.



From the original questioner:
Thanks all for the responses. This first commercial job is going to be very interesting and I'm actually excited about it. It's like back in the day when this was a hobby and actually fun! I liked the Blum system the best. It was exactly what I was looking for, for the time being. I guess I will find out for sure when the job is over.


From contributor W:
The boring patterns will be the easy part. Wait until you get into submittals, getting paid, filing liens, etc.


From contributor L:
If you are running on a CNC, you can dump the 32 balanced system and move on. We fabricate and install thousands of cabinets yearly. I run a slider, ptp and bander. We use two thicknesses of stock - 1/4" for backs and bottoms and 3/4" for everything else, period. Our hanging cleats are basically from off-fall and so are the drawer sides.

Whatever you do, don't try and convince the GC or the architect.

I had purchased a couple of jobs from Cab Parts and just hated their count from this and that and that is where the slide goes or hinges or whatever. So I bought a ptp, slider and bander and made my own system. Believe me, I do not pay anyone to count holes to put hinges and slides where they belong. Our doors roll up to a Blum hinging machine and we drill and press all at once.

Because you are programming a machine, you can pick and choose where hardware goes. When we drill for a 4 drawer base, we drill for construction, stretcher and hardware, and the placement of hardware takes seconds because there are only holes for the hardware.

You need to think engineered cases, not 32 system. The only relation 32mm has for you is that is the spacing for hardware and shelf adjustment holes. Don't waste your precious money drilling for what you don't need. Others that are running gang drills are correct with what they own, but what you own is a different beast.

We have 8 spindles on our line boring block. We only drill for the exact amount of shelf pins that is efficient so we can get the next part on the machine. I will not waste my money drilling for a balanced panel. Some of the blueprints I get have a drawing for 11 adjustment holes in an upper of 30" tall and 7 for a base; that's all they get. When I produce shop drawings for jobs, I show less than that, and that is what they get. Period.

Something else, along the lines of shelf holes and hinges - I drill 37mm back for hinge plate placement at the same distance from each edge - parametric, and if the length of the end changes, we can make the change at the machine and it always remains the same. For the adj holes I drill at 50mm back and therefore no one can confuse what is a hinge plate placement set of holes and what is shelf holes.