Residue-Free Labels Latest in Tools and Supplies

Melisi Compared To Ilva

02/02/2015


From original questioner:

What are ur guys thoughts, durability and final product of Melisi LRK 181 compared to ilva?

Melisi is out of my price range.

Im spraying out of a Binks Rapitor.

From contributor he


you may not believe this but the are owned by the same company, products are very close to be the equal of each other

good luck

herb j

From contributor Mi


I just spoke to a company from whom we buy touch up and refinishing supplys from and they sell this and its hundreds less than Melisi

From contributor he


hard to figure the thinking behind the pricing, was shocked when i found out

From contributor Ri


I've used both and liked the Milesi sealer a little better but have no problem with Ilva products and we're using a ton of it right now.

From contributor Mi


Thx and herb but im more soecifically refering to their arcylic poly 2k paint that is a primer/paint all in one.from my understanding, with Ilva, it's a 2:1 ratio paint to catalyst, which seems like a lot compared to melisi, but if memory serves, its 32oz of paint to 10 oz of catalyst, so in the immediate term its less to get ilva, but i think long term its more expensive for ilva. But actual costs of ilva to melisi, i think ilva is cheaper, so it may be about the same at the end if the day

From contributor Je


Mike, I am the GM for Milesi North America please feel free to contact me at Milesi@milesi.us.

From contributor Da


The Ilva High Performance Acrylic products are composed of a 2 component water white ( non yellowing) undercoat TA00012. Catalyzed at 20% with TX90. Thin with slow TZ13.
The 2K topcoat TS series. We have 6 Gloss levels in stock 5/15/25/35/50/65. Our 100 gloss "Italian wet look" is TP11.
A new High-scratch resistance Techno topcoat finish TS in 7 sheens from 5 through 65 gloss.
Also Available is an acrylic dead matte self sealer TS18.
All contain a UV inhibitors and all the above are in stock.
If you need any further information regarding these or any other ILVA coatings.
Please contact me.
David Bartholomey ILVA ICS.