Knife Planing Across the Grain Can be Applied to Hardwoods

Shows that knife planing across the grain can be applied to most domestic hardwood species to produce a satisfactory finish knife-planed surface and flakes for particleboard. 1975
This article is in PDF format (file size: 1645 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Knife Planing Across the Grain Can be Applied to Hardwoods   (1975)

Shows that knife planing across the grain can be applied to most domestic hardwood species to produce a satisfactory finish knife-planed surface and flakes for particleboard.

Author: Stewart, Harold A.


Source: Research Note NC-196. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Stewart, Harold A.  1975.  Knife Planing Across the Grain Can be Applied to Hardwoods  Research Note NC-196. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.