Energy requirements for lumber drying kilns can depend on kiln size and range from 18,000 Btu/lb water evaporated for a 10 board food capacity kiln to 1,600 Btu/lb water evaporated for a 100,000 board foot capacity kiln. 1980
This article is in PDF format (file size: 282 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Kiln Size Affects Energy Required to Dry Lumber   (1980)

Energy requirements for lumber drying kilns can depend on kiln size and range from 18,000 Btu/lb water evaporated for a 10 board food capacity kiln to 1,600 Btu/lb water evaporated for a 100,000 board foot capacity kiln.

Author: Rosen, Howard N.


Source: Research Note NC-256. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station