Hardwood siding performance

A 6-year exposure test of three styles of siding made from nine hardwoods and given three treatments showed that full-length yellow-poplar vertical tongue-and-groove siding dip-treated in a water-repellent preservative performed best. 1967
This article is in PDF format (file size: 5892 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Hardwood siding performance.   (1967)

A 6-year exposure test of three styles of siding made from nine hardwoods and given three treatments showed that full-length yellow-poplar vertical tongue-and-groove siding dip-treated in a water-repellent preservative performed best.

Author: Cooper, Glenn A.


Source: Research Paper NC-16. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Cooper, Glenn A.  1967.  Hardwood siding performance.   Research Paper NC-16. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.