Suggestions for adhering closed-cell PVC panel goods to a wood substrate. November 30, 2009

Question
Does anyone know of a quick-set glue to bond plastic (sintra) to wood?

Forum Responses
(Adhesive Forum)
From contributor D:
Back when I was in film set construction we'd use sintra as easy white stage floors. We'd rough up the back (say 80 grit) and stick it down to the substrate with solvent-based contact cement. It stuck forever!



From contributor J:
Locktite power grab works well. It is not "instant" as advertised, but if you apply and cure 24 hours above 57 degrees it will work.