Field identification of birdseye in sugar maple (Acer saccharum Marsh.)

Gives procedures for the field identification of birdseye in standing sugar maple (Acer saccharum Marsh.) trees. 1994
This article is in PDF format (file size: 13143 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Field identification of birdseye in sugar maple (Acer saccharum Marsh.)   (1994)

Gives procedures for the field identification of birdseye in standing sugar maple (Acer saccharum Marsh.) trees.

Author: Bragg, Don C.; Stokke, Douglas D.


Source: Research Paper NC-317. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Bragg, Don C.; Stokke, Douglas D.  1994.  Field identification of birdseye in sugar maple (Acer saccharum Marsh.)  Research Paper NC-317. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.