Residue-Free Labels Latest in Tools and Supplies

Effects of Stock Removal Rates on Belt Loading for Abrasive Planing Hardwoods

Belt loading increases up to a point and then decreases as stock removal rate increases for red oak and yellow-poplar 1978
This article is in PDF format (file size: 1039 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Effects of Stock Removal Rates on Belt Loading for Abrasive Planing Hardwoods   (1978)

Belt loading increases up to a point and then decreases as stock removal rate increases for red oak and yellow-poplar

Author: Stewart, Harold A.


Source: Research Note NC-240. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Stewart, Harold A.  1978.  Effects of Stock Removal Rates on Belt Loading for Abrasive Planing Hardwoods  Research Note NC-240. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.