Freshly sawn boards and stem cross-sectional disks, 4/4 and 8/4 thick, of three hardwood species were dried at six indoor and outdoor household locations in southern Illinois. It took silver maple and black cherry 90 days and white oak from 90 to 150 days to dry to less than 10% moisture content at the indoor locations. 1982
This article is in PDF format (file size: 2567 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Drying small quantities of green hardwoods at home.   (1982)

Freshly sawn boards and stem cross-sectional disks, 4/4 and 8/4 thick, of three hardwood species were dried at six indoor and outdoor household locations in southern Illinois. It took silver maple and black cherry 90 days and white oak from 90 to 150 days to dry to less than 10% moisture content at the indoor locations.

Author: Miceli, Charles M.; Rosen, Howard N.; Spalt, Howard A.


Source: Research Paper NC-228. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station

Citation: Miceli, Charles M.; Rosen, Howard N.; Spalt, Howard A.  1982.  Drying small quantities of green hardwoods at home.  Research Paper NC-228. St. Paul, MN: U.S. Dept. of Agriculture, Forest Service, North Central Forest Experiment Station.