Residue-Free Labels Latest in Tools and Supplies

Determining Wood EMC -- (Equilibrium Moisture Content)

Other Versions
Spanish
How to calculate and establish EMC. From the Forest Products Laboratory. February 16, 2004

This publication by the Forest Products Laboratory provides information on how to determine the wood equilibrium moisture content (EMC) for given location or environment. Tables include: calculating EMC based on known relative temperature and humidity, and calculating EMC based on geographical location.

To view the file, left click the link below. To download the file, right click and choose "save target as". The document is in Acrobat PDF format. Download latest Acrobat Reader if required.

Determining Wood Equilibrium Moisture Content (EMC) (PDF 555 KB)