Current trends in the management of aspen and mixed aspen forests for sustainable production

Quaking aspen (Populus tremuloides Michx.) is a remarkable species that performs several significant ecological roles throughout its range while at the same time is facing ever-increasing harvesting pressure. Although its full product potential remains untapped, aspen utilization has increased noticeably in the past 15 years as it has become a desired species for engineered wood products such as oriented strand board, and a preferred hardwood in the production of high quality pulp and paper products. Concurrent with this increase in aspen utilization has been an increase in the importance of ecological concepts must be grounded in the silvics and life history traits of the species. Here we present three trends in aspen management; aspen retention, a renewed interest in aspen thinning, and the advent of cut-to-length (CTL) harvesters that allow forest managers to address these considerations by capitalizing on aspen`s unique characteristics. Finally, we discuss traditional harvesting methods and these trends in the context of their genetic implications. 2001
This article is in PDF format (file size: 3002 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Current trends in the management of aspen and mixed aspen forests for sustainable production   (2001)

Quaking aspen (Populus tremuloides Michx.) is a remarkable species that performs several significant ecological roles throughout its range while at the same time is facing ever-increasing harvesting pressure. Although its full product potential remains untapped, aspen utilization has increased noticeably in the past 15 years as it has become a desired species for engineered wood products such as oriented strand board, and a preferred hardwood in the production of high quality pulp and paper products. Concurrent with this increase in aspen utilization has been an increase in the importance of ecological concepts must be grounded in the silvics and life history traits of the species. Here we present three trends in aspen management; aspen retention, a renewed interest in aspen thinning, and the advent of cut-to-length (CTL) harvesters that allow forest managers to address these considerations by capitalizing on aspen`s unique characteristics. Finally, we discuss traditional harvesting methods and these trends in the context of their genetic implications.

Author: David, A. J.; Zasada, John C.; Gilmore, D. W.; Landhausser, S. M.


Source: Forestry chronicle. Vol. 77, no. 3 (May/June 2001).:p. 525-532.

Citation: David, A. J.; Zasada, John C.; Gilmore, D. W.; Landhausser, S. M.  2001.  Current trends in the management of aspen and mixed aspen forests for sustainable production  Forestry chronicle. Vol. 77, no. 3 (May/June 2001).:p. 525-532..