Wall Angle °
38/52 miter 38/52 bevel 45/45miter 45/45 bevel
1
89.18 51.99 89.29 44.99
2
88.37 51.98 88.58 44.99
3
87.56 51.97 87.87 44.98
4
86.75 51.95 87.17 44.96
5
85.94 51.93 86.46 44.94
6
85.13 51.89 85.76 44.92
7
84.32 51.86 85.05 44.89
8
83.52 51.82 84.35 44.86
9
82.71 51.77 83.64 44.82
10
81.91 51.72 82.94 44.78
11
81.11 51.66 82.24 44.73
12
80.31 51.60 81.54 44.68
13
79.51 51.53 80.84 44.63
14
78.72 51.45 80.14 44.57
15
77.92 51.37 79.45 44.51
16
77.14 51.29 78.75 44.44
17
76.35 51.20 78.06 44.37
18
75.57 51.10 77.37 44.29
19
74.79 51.00 76.68 44.21
20
74.02 50.89 75.99 44.13
21
73.24 50.78 75.31 44.04
22
72.47 50.67 74.62 43.95
23
71.71 50.55 73.94 43.86
24
70.95 50.42 73.26 43.76
25
70.19 50.29 72.59 43.65
26
69.44 50.15 71.91 43.54
27
68.69 50.01 71.24 43.43
28
67.95 49.87 70.57 43.32
29
67.21 49.72 69.91 43.20
30
66.48 49.56 69.24 43.07
31
65.75 49.40 68.58 42.95
32
65.02 49.24 67.92 42.82
33
64.30 49.07 67.27 42.68
34
63.59 48.90 66.61 42.54
35
62.88 48.72 65.96 42.40
36
62.17 48.54 65.32 42.26
37
61.47 48.35 64.67 42.11
38
60.78 48.16 64.03 41.95
39
60.09 47.97 63.39 41.80
40
59.40 47.77 62.76 41.64
41
58.73 47.57 62.13 41.47
42
58.05 47.36 61.50 41.31
43
57.38 47.15 60.87 41.14
44
56.72 46.93 60.25 40.96
45
56.06 46.72 59.63 40.78
46
55.41 46.49 59.02 40.60
47
54.76 46.27 58.41 40.42
48
54.12 46.04 57.80 40.23
49
53.49 45.81 57.19 40.04
50
52.85 45.57 56.59 39.85
51
52.23 45.33 55.99 39.65
52
51.61 45.09 55.40 39.46
53
50.99 44.84 54.81 39.25
54
50.38 44.59 54.22 39.05
55
49.78 44.34 53.64 38.84
56
49.18 44.08 53.05 38.63
57
48.59 43.83 52.48 38.41
58
48.00 43.56 51.90 38.20
59
47.42 43.30 51.33 37.98
60
46.84 43.03 50.76 37.76
61
46.26 42.76 50.20 37.53
62
45.69 42.48 49.64 37.30
63
45.13 42.21 49.08 37.07
64
44.57 41.93 48.53 36.84
65
44.0 41.65 47.98 36.61
66
43.47 41.36 47.43 36.37
67
42.92 41.08 46.89 36.13
68
42.38 40.79 46.35 35.88
69
41.85 40.49 45.81 35.64
70
41.32 40.20 45.28 35.39
71
40.79 39.90 44.75 35.14
72
40.27 39.60 44.22 34.89
73
39.76 39.30 43.69 34.63
74
39.24 39.00 43.17 34.38
75
38.74 38.69 42.66 34.12
76
38.23 38.38 42.14 33.86
77
37.74 38.07 41.63 33.59
78
37.24 37.76 41.12 33.33
79
36.75 37.44 40.62 33.06
80
36.26 37.13 40.12 32.79
81
35.78 36.81 39.62 32.52
82
35.30 36.49 39.12 32.25
83
34.83 36.17 38.63 31.97
84
34.36 35.84 38.14 31.70
85
33.89 35.51 37.65 31.42
86
33.43 35.19 37.17 31.14
87
32.97 34.86 36.69 30.85
88
32.51 34.53 36.21 30.57
89
32.06 34.19 35.73 30.28
90
31.61 33.86 35.26 30.00
91
31.17 33.52 34.79 29.71
92
30.73 33.19 34.32 29.41
93
30.29 32.85 33.86 29.12
94
29.86 32.50 33.40 28.83
95
29.43 32.16 32.94 28.53
96
29.00 31.82 32.48 28.23
97
28.57 31.47 32.03 27.93
98
28.15 31.13 31.57 27.63
99
27.73 30.78 31.12 27.33
100
27.32 30.43 30.68 27.03
101
26.90 30.08 30.23 26.73
102
26.49 29.73 29.79 26.42
103
26.09 29.37 29.35 26.11
104
25.68 29.02 28.92 25.80
105
25.28 28.66 28.48 25.49
106
24.88 28.31 28.05 25.18
107
24.49 27.95 27.62 24.87
108
24.09 27.59 27.19 24.55
109
23.70 27.23 26.76 24.24
110
23.32 26.87 26.34 23.92
111
22.93 26.50 25.91 23.61
112
22.55 26.14 25.49 23.29
113
22.17 25.78 25.08 22.97
114
21.79 25.41 24.66 22.65
115
21.41 25.05 24.25 22.33
116
21.04 24.68 23.83 22.00
117
20.6 24.31 23.42 21.68
118
20.30 23.94 23.02 21.35
119
19.93 23.57 22.61 21.03
120
19.56 23.20 22.20 20.70
121
19.20 22.83 21.80 20.37
122
18.84 22.45 21.40 20.04
123
18.48 22.08 21.00 19.71
124
18.12 21.71 20.60 19.38
125
17.77 21.33 20.20 19.05
126
17.41 20.96 19.81 18.72
127
17.06 20.58 19.42 18.39
128
16.71 20.20 19.02 18.05
129
16.36 19.83 18.63 17.72
130
16.01 19.45 18.24 17.38
131
15.67 19.07 17.86 17.05
132
15.32 18.69 17.47 16.71
133
14.98 18.31 17.09 16.37
134
14.64 17.93 16.70 16.03
135
14.30 17.55 16.32 15.69
136
13.97 17.17 15.94 15.36
137
13.63 16.79 15.56 15.02
138
13.30 16.40 15.19 14.68
139
12.96 16.02 14.81 14.33
140
12.63 15.64 14.43 14.00
141
12.30 15.25 14.06 13.65
142
11.97 14.87 13.68 13.31
143
11.64 14.48 13.31 12.97
144
11.31 14.09 12.94 12.62
145
10.99 13.71 12.57 12.28
146
10.66 13.32 12.20 11.93
147
10.33 12.93 11.82 11.58
148
10.01 12.55 11.46 11.23
149
9.69 12.16 11.10 10.89
150
9.36 11.78 10.72 10.54
151
9.04 11.37 10.36 10.19
152
8.72 10.98 9.99 9.84
153
8.40 10.60 9.63 9.50
154
8.08 10.21 9.27 9.15
155
7.77 9.82 8.90 8.80
156
7.45 9.42 8.54 8.45
157
7.13 9.03 8.19 8.10
158
6.82 8.64 7.82 7.75
159
6.51 8.26 7.46 7.40
160
6.19 7.86 7.10 7.05
161
5.88 7.47 6.74 6.70
162
5.56 7.08 6.39 6.35
163
5.25 6.68 6.03 6.00
164
4.95 6.29 5.67 5.64
165
4.63 5.90 5.32 5.29
166
4.32 5.51 4.96 4.94
167
4.01 5.11 4.60 4.59
168
3.70 4.72 4.25 4.23
169
3.39 4.33 3.89 3.88
170
3.08 3.93 3.54 3.53
171
2.77 3.54 3.18 3.18
172
2.46 3.15 2.83 2.83
173
2.15 2.75 2.47 2.47
174
1.84 2.36 2.12 2.12
175
1.53 1.96 1.76 1.76
176
1.23 1.57 1.41 1.41
177
.92 1.18 1.06 1.06
178
.62 .79 .71 .71
179
.30 .39 .35 .35