Residue-Free Labels Latest in Tools and Supplies

Converting A Shipping Container to a Drying Kiln

Other Versions
Spanish
Design, construction, and operation info from folks who've done it. February 26, 2005

Question
Has anyone had any experience with converting an overseas shipping container to a DH kiln?

Forum Responses
(Sawing and Drying Forum)
From contributor D:
Yes, it is very commonly done. You must use a refrigerated container to get the level of insulation that you need. A 40' hi cube, when properly set up as a kiln, will hold about 5000 board feet (12M3). The size of the dehumidifier depends on the species and thickness being dried.



From contributor C:
Here is one I'm building out of a 40' container. After I install the misting system, I'm having the inside sprayed with 4" of polyurethane foam. I wish I had used a high cube for more head space. I should be able to load 3000 - 4000 bdft. I only have two 16' kiln carts, so I'm not utilizing all the possible space.




From contributor P:
I use an old 1968 Trailer mobil meat hauling refer for a workshop. I heat it with a forced air heat and once it is warmed up in the winter, the heat holds very well, so for a hot kiln I bet holding high temps could be easier than a stick built kiln. I was lucky to get such a nice interior walled unit, foam under fiberglass panels. I found a trailer dealer locally that sold used and new trailers. I have had mine 14 years and have about $1K invested after I repaired both door systems. Shop around before buying the first thing you see. Look around salvage yards, too - sometimes an exterior crash-damaged trailer can be bought for a few hundred dollars.



From the original questioner:
What kind of a forced air unit are you using and where did you install the unit? Do you have fans installed in it?


From contributor P:
I have a 50K propane heater suspended from the ceiling (halfway back). It works good for me and I use a carbon monoxide detector for safety (mandatory, I'd say). It has its own internal fan. These type refer units are very air tight, I've found, so they hold heat or cold very well indeed.


From contributor G:
If you are not using all the available space, then you need to baffle it off. Looks like you are going to use two kiln carts end on end. If this is the case, then I think you will need more fans. I could see only maybe three in the picture. Got to have good, even air flow through the stack for proper drying. Looks like you are going to have a pretty nice kiln once you get it done.


From contributor C:
I used four fans and I will be baffling all the unused space for maximum air flow through the piles.


From contributor G:
I have found that three fans in a 16 foot DH kiln work real good. Anything less than that seems to give me uneven drying.


From contributor S:
I have a 45' hi cube shipping container kiln, with a Nyle 200 dehumidification unit and Wood-Mizer controller. Here are some of my lessons learned:

1. Purchase an insulated container if at all possible. High cube (9.5' ceiling height) is the best way to go. A 45' length will let you get two carts of 16' cants and one cart of 12' cants in the kiln, which works out to around 4500 bf.

2. If you can't get an insulated container, the following process is very effective: Glue 1" foamboard (R3.2) to the inside top, sides and ends of the container. Over this, glue FBBWP (foil, bubble, bubble, white poly) Tekfoil available from FarmTek (www.farmtek.com). It's about 3/8" thick, and has an R value of 10.

This insulation combination is unbelievably effective at retaining heat inside the kiln, and moisture will not easily condense on the white poly. On a seventy degree day, with an inside kiln temperature of 120 degrees, the steel outer shell of my container is about 72 degrees.

3. Build a track system inside the kiln, and even more importantly, extend the tracks outside the kiln. You will need to have about a 4' removable gap between the kiln and the outside tracks to allow the doors to close. The Nyle manual provides an example of an effective track system. Don't skimp on your kiln carts or cart wheels.

Inside track is important because the weight of the lumber can punch the cart wheels right through the wood floor of the container. Track outside the kiln is critical in order to use a forklift or tractor loader to load the kiln carts.

4. Build a relief in the side of the container for the dehumidification unit to sit in. It provides for more consistent air flow through the kiln and you reduce the chance of damaging your dehumidifier during loading or load inspections.

5. Install one fan for every 8 feet of container length. I have 5 in my 45' container. Hang the fans on rubber mounts (Grainger’s has them), otherwise the steel container will reverberate and you'll hear it humming 600' away.

6. If you live in a rural area that is subject to power outages or surges (such as when a tree strikes a power line), be sure to install a surge arrestor on your load center. The kiln controllers can be susceptible to voltage surges. You can get surge arrestors at an electrical supply center.

7. If you purchase a Nyle unit, consider ordering the extended length cable from the controller to the dehumidifier. The standard 6' length is a little short.

8. Clean and paint all exposed metal surfaces inside the container, as moisture will condense and the metal will rust quickly. This is especially important on the insides of the doors and bottom of the door frame.

The folks at Nyle are really great, and their products are top quality and reasonably priced.

I have about 11k invested in my container kiln, excluding labor. Breakdown is as follows:

Container, delivered: 1,500.00
Nyle (Wood-Mizer) 200 series kiln: 4,745.00
Three extra fans (Nyle): 725.00
Moisture meter: 410.00


Steel for kiln carts and tracks: 1,000.00
Kiln cart wheels (Nyle): 420.00
Insulation (1" foam) 45 sheets @ 13.00 ea: 585.00
Insulation (Tekfoil FBBWP) 1,500 sq. ft.: 600.00
Misc electrical (load ctr, boxes, wiring): 350.00
Plywood and hinges for baffles: 350.00
Misc hardware: 100.00
Metal and wood for side kiln chamber: 200.00

Total, excluding labor: 10,985.00

From a labor perspective, it took the following: Two men about 40 hours to glue in the insulation, with furring strips for extra support, and to build the side kiln chamber. It took two men about 40 hours to install the fans (including electrical) and fabricate the plywood baffles. Finally, it took two men about 50 hours to fabricate three kiln carts (two 16' carts, and one 12' cart), and the track system inside and outside the kiln.