Residue-Free Labels Latest in Tools and Supplies

Cherry Lumber Defects

08/17/2015


From original questioner:

Are the very darkest spots on this cherry a defect? It it some kind of fungus or rot?

From contributor ri


looks like the surface oxidation from kiln drying didn't clean up. Needs another pass in you Dewalt there.

From contributor Ri


Thanks for responding. That not my lumber or Dewalt. I was asked by the owner of the lumber what the spots are I didn't really know.

From contributor do


You will see more spots like that in 1 common cherry.
I dont know what they are but that is why i use select&better.

From contributor Jo


Looks like pitch pockets. This is a natural characteristic of Cherry lumber and is not a defect in the low end grades. That is why I only buy FAS or proprietary graded lumber so that these defects are graded out of the lumber along with the SAP wood.