Residue-Free Labels Latest in Tools and Supplies

BEADED PROFILE IN PVC

05/13/2014


From original questioner:

Can anyone help me figure out which tool to use for wanescoating or beaded profile in PVC?

thanks,

LH

From contributor De


A saw type cutter will work great assuming you have a saw or molder head. Router bits will work but you will need a flat at the bottom as anything with a point in a router bit will just make a mess of things. The picture is of one of many custom cutters I have had made over the years.

From contributor st


Here is a Magic Molder profile we have used. They make different sized ones.
We run it on a table saw.

From contributor Lu


Dean and all who have responded,

Thanks a lot for the help.

-Luke

From contributor Za


Amana or Whiteside makes a bit that I have used before. It dosen't come to a point, but the flat area was minimal.