Shop-Built Cove Table

Listing #161   Listed on: 03/01/2016
Built this table around a cove rod for postform backsplashes. Wired in a warning light as well.
(No images available for this Shopbuilt Equipment listing.)
Viewer Comments:


Posted By: Lee     [05/09/2016]
Where did you get the cove rod? Do you have a timer on it? Or do you use templiq crayon to know when it's ready?


Posted By: Pazzulla     [05/10/2016]
I bought the cove rod, isolators, and a rheostat switch from schultzform out here in California. No timer or templiq. Just bend it by feel.


Posted By: Alien     [05/21/2016]
How do you like your slot former I see in the back? Can you do waterfall edge or just bullnose? I was thinking about building one.


Posted By: Pazzulla     [05/23/2016]
Slotformer is awesome. I also got that from schultzform in Socal. It does 180 wrap, waterfall, radius/flat/radius, bullnose. Its adjustable to around 4".


Posted By: DawidPotul     [06/20/2016]
Awesome.


Add your comment (* denotes required fields):
* Your Name:
* Your Email:
  * Enter your comment below:
*Enter the correct numbers into the field below:
  I have read WOODWEB's Site User Agreement
  (Submitted comments may be edited for clarity)

Date of your Birth: