Walnut and Hard Maple finished with hand rubbed Waterlox. Two piece set; top has coat hanger and cowboy hat rack. Bottom has two hidden drawers and cabinet door to appear hidden. Cabinet panels are full floating, hand made plywood. The only hardware is the door hinges. All components and joints are hand made.
Viewer Comments:
I like the wall unit, can you tell me why handmade plywood, and why small drawers instead of using the entire box ?
I use hand made plywood for the panels to minimize expansion. I wanted the drawers to be of the same size and to appear hidden. The size of drawer would of course be to the customers request. How much "stuff" does a man have to at his ready for getting dressed?
Nice ! Every man knows you need one of those hidden compartments, hide extra money :)