Description
1999 Motionmaster Router, three heads:
1-15hp and 3/4 collet,1- 7.5 hp 1/2" collet,1- 3hp Porter Cable router mounted horizontally for tenoning
or the third head can be a pneumatic drill head w 3/8" chuck (drills down in Z direction). 440v (transformer 220v to 440v available.
Table 60" x 60". Weighs 8,000 lbs,7'-8" wide, 8' long, 4'-6" high, can load out. High speed travel up to 500 ipm. Operates on standard G & M codes, Fagor 8055 controller new 2013. Fagor is one of the standard controllers and reads over eighty common G and M codes as well as program flow commands in the BASIC language for looping, cutting and counting multiple parts, to wait for operator input, and if then statements.. 3 hp Vacuum pump and table. Stack of manuals and reference books included. Remote terminal (Windows PC) included, can operate router through terminal (drip feed large files, file editing, file management easier. Full look ahead and 3d machining. Was used to scoop chair seats, 3 mins per seat @ 1/8"
stepover, 1" scoop depth. 500 ipm actual rapid travel.
Vacuum table (under spoilboard in picture) has a grid machined for holding parts anywhere on the table.
Used manufacturing chairs, a real beast, not a lightweight shop router. Business (nwchairs) closed last year.
Basic operational training included.