Description
OMGA Optima 120 4200 CE Push Feed Optimizing and Defecting Cut-Off Saw (2021)
208v, 7.38 kW, 60 Hz, 3PH
Maximum mm: 500 PH
Minimum mm: 400 PH
Bore mm: 35 mm
Maximum piece thickness: 4-5/16"
Maximum piece width: 12"
Maximum infeed length: 13'9" or 20'4"
Maximum feed speed: 400 fpm
Saw blade motor power: 6HP
Saw blade diameter: 18" (20" opt)
Feed motor power: 2.7 Nv (1.50 kW)
Cutting speed: 0.4-2 second
Average number of cuts: 25-35 min.
Touch screen operated
Push button controls
For additional technical specifications please refer to above PDF
Includes 46" x 240" sorting table
Includes (5) kickoffs
Elca 3-Phase Transformer
20 kVA, 60 Hz, ta.40 degrees C
Input: 208v, 60 AT
Output: 480v, 25A
Class 155 degrees C